FORESTERITE BRICK, REBONDED FUSED-MAGNESIA BRICK |
|
index
item |
foresterite brick |
rebonded fused magnesia brick |
MgO% min |
60 |
60 |
95 |
97 |
SiO 2 % min |
20 |
20 |
¡Ý2.0 |
¡Ý1.5 |
0.2MPa refractoriness under load 0 C min |
1650 |
1600 |
1700 |
1700 |
cold crushing strength MPa min |
40 |
35 |
45 |
45 |
apparent porosity% max |
20 |
21 |
18 |
18 |
thermal shock resistance (9500 0 C-air) times max |
10 |
7 |
- |
- |
bulk density g/cm 3 min |
2.70 |
2.65 |
- |
- |
hot bending strength MPa min |
- |
- |
The test data shall be noted in the qulity certificate |
|